SEGREGATION OF SOLUTE ELEMENTS IN CRUCIBLE DURING DIE CASTING
Abstract
In this work, the segregation of solute elements in magnesium alloys AZ91D and AM60B in a crucible during hot-chamber die casting process has been investigated. The sampling of molten metal for chemical composition analysis was carried out at three positions within a crucible of 600 mm in depth. The picked molten metal was poured into a steel mold to cast into a rod 40mm diameter and 120mm length.
About the Authors
Keun Yong SohnKorea, Republic of
Dept. of Advanced Materials Research
Kang Min Cheol
Korea, Republic of
Kyung Hyun Kim
Korea, Republic of
Dept. of Advanced Materials Research
References
1. Brown R., Magnesium Technology 2000 ed. by Kaplan H.I., Hryn J„ Clow B., 2000 TMS, March 12-16, NashviUe, Tennessee, USA, 2000, P.3. '
2. Sohn K.Y., Kang M.C., Kim K.H. Mat. Sci. Forum. 2003. Vol. 419-422, P.135.
3. Hanwait J.D. et al. Trans AIME. 1942. Vol. 147, P.273.
Review
For citations:
Sohn K.Y., Cheol K.M., Kim K.H. SEGREGATION OF SOLUTE ELEMENTS IN CRUCIBLE DURING DIE CASTING. Litiyo i Metallurgiya (FOUNDRY PRODUCTION AND METALLURGY). 2005;(3):58-61.