INFLUENCE OF THE REGIMES OF COOLING OF THE ROLLED WIRE WITH DIAMETER 5,5-9,0 MM OF LOW-CARBON TYPES OF STEEL AT THE MILL 150 AND OF STORAGE DURATION ON STRIPPABILITY OF CINDER IN MECHANICAL WAY

Abstract

This work is dedicated to investigation of peculiarity of cinder formation on rolled wire in the process of its cooling immediately after rolling, of the factors influencing on strippability of cinder at testing of the rolled wire samples after rolling and also after 20 and 50 days of storing outdoors.

About the Author

N. V. Voronov
Byelorussian Steel Works
Belarus


References

1. ДелюстоЛ. г. Абразивно-порошковая очистка проката от окалины М.: Машиностроение, 2002.

2. Луценко В. А. Влияние параметров высокоскоростной термомеханической обработки на процессы окалинообразования углеродистой стали // Литье и металлургия. 2005. №2. 4.2. С. 96-98.


Review

For citations:


Voronov N.V. INFLUENCE OF THE REGIMES OF COOLING OF THE ROLLED WIRE WITH DIAMETER 5,5-9,0 MM OF LOW-CARBON TYPES OF STEEL AT THE MILL 150 AND OF STORAGE DURATION ON STRIPPABILITY OF CINDER IN MECHANICAL WAY. Litiyo i Metallurgiya (FOUNDRY PRODUCTION AND METALLURGY). 2005;(3):103-106. (In Russ.)

Views: 303


Creative Commons License
This work is licensed under a Creative Commons Attribution 4.0 License.


ISSN 1683-6065 (Print)
ISSN 2414-0406 (Online)