VERTICAL CENTRIFUGAL CASTING OF A HYPEREUTECTIC SILUMIN WITH COOLING OF THE MOLD AND CASTING

https://doi.org/10.21122/1683-6065-2017-2-5-11

Full Text:

Abstract

It is shown that cooling of casting molds by water with water flow of 0,42 m3/h and internal surfaces of castings with thickness of a wall 12–14 mm with water quantity 2,5×10–4–5×10–4 m3 allows to receive procurements with completely modified microstructure without use of modifiers. External layers of the produced castings consist of the eutectic silumin with compact crystals of silicon, and internal layers – of hypereutectic silumin with crystals of high-disperse primary and compact eutectic silicon.

For citations:


Marukovich E.I., Stetsenko V.Yu., Baranov K.N. VERTICAL CENTRIFUGAL CASTING OF A HYPEREUTECTIC SILUMIN WITH COOLING OF THE MOLD AND CASTING. Litiyo i Metallurgiya (FOUNDRY PRODUCTION AND METALLURGY). 2017;(2):5-11. (In Russ.) https://doi.org/10.21122/1683-6065-2017-2-5-11

Views: 695


Creative Commons License
This work is licensed under a Creative Commons Attribution 4.0 License.


ISSN 1683-6065 (Print)
ISSN 2414-0406 (Online)