PECULIARITIES OF STRUCTURE FORMATION OF THE CONSTRUCTIONAL ALLOYED STEEL AT HEAT TREAT MENT OF HIGHQUALITY ROLLED IRON
Abstract
The structure formation in electric steel 42Cr4Mo2 under continuous cooling is investigated, the results are summarized in the form of the thermo-kinetic diagram. It is shown that rolled metal annealing during 3.5-4.0 hours at 650-680°C provides the necessary properties of steel and enables to maintain energy consumption.
About the Authors
V. A. LutsenkoUkraine
P. A. Bobkov
Belarus
T. N. Golubenko
Ukraine
L. A. Drobyshevsky
Belarus
V. I. Gritsayenko
Belarus
Review
For citations:
Lutsenko V.A., Bobkov P.A., Golubenko T.N., Drobyshevsky L.A., Gritsayenko V.I. PECULIARITIES OF STRUCTURE FORMATION OF THE CONSTRUCTIONAL ALLOYED STEEL AT HEAT TREAT MENT OF HIGHQUALITY ROLLED IRON. Litiyo i Metallurgiya (FOUNDRY PRODUCTION AND METALLURGY). 2013;(1):38-42. (In Russ.)