Abstract

The article describes the experience of using deoxidizing powder in the technological process of production of hot-rolled seamless pipes; the processes that occur when applying to the inner surface of the hollow billet deoxidizing powder. The results of experimental and industrial tests of deoxidizing powder of different chemical composition are presented. The influence of the chemical composition of the deoxidizing powder on the formation of defects on the inner surface of the pipes is shown. Describes the stages of metallographic analysis of the defects on the inner surface of the pipe, provided the reasons for the formation of the defect «pipe rolling lap (skin)».

About the Author

O. V. Rozhkova
BSW - management company of "BMC" holding
Belarus
Zhlobin city, Gomel region, Belarus, 37, Promyshlennya str


References

1. Gol’dshtejn M. I., Grachev S. V., Veksler Ju. G. Special’nye stali [Special steels]. Moscow, Metallurgija Publ., 1985, 408 p.


Review

For citations:


Rozhkova O.V. Influence of deoxidizing powder on the internal surface of hot-rolled pipes. Litiyo i Metallurgiya (FOUNDRY PRODUCTION AND METALLURGY). 2019;(1):61-65. (In Russ.) https://doi.org/10.21122/1683-6065-2019-1-61-65

Views: 2198


Creative Commons License
This work is licensed under a Creative Commons Attribution 4.0 License.


ISSN 1683-6065 (Print)
ISSN 2414-0406 (Online)