Changing the mechanical characteristics of cracking pipes during their long‑term operation
https://doi.org/10.21122/1683-6065-2025-2-64-70
Abstract
The article presents the results of a study on the strength characteristics (tensile strength) of cracking pipes after prolonged operation. It was found that the strength properties of the pipe material deteriorated, while plasticity characteristics showed a slight increase. The decrease in conditional yield strength reached 39.94 %, and the reduction in tensile strength was 40.05 %. It was established that specimens taken from the used pipe underwent 25 % more elongation before fracture compared to specimens made from a new pipe. Using thermomechanical coefficients, the expected values of true yield strength for both materials were calculated. The results showed that the true yield strength of the used pipe material differs significantly from tabulated values, suggesting that for strength assessment of such structures, the true σT should be determined experimentally. If theoretical approaches are used, the influence of operational time on changes in mechanical properties of the metal must be taken into account.
About the Authors
S. V. PilipenkoBelarus
Novopolotsk, Belarus, 29, Blokhina str.
A. V. Dudan
Belarus
Novopolotsk, Belarus, 29, Blokhina str.
O. P. Shtempel
Belarus
Novopolotsk, Belarus, 29, Blokhina str.
T. V. Vigerina
Belarus
Novopolotsk, Belarus, 29, Blokhina str.
References
1. Chirkova A. G., Mahutov N.A., Kuzeev I. R., Gafarova V.A. Raschetno‑jeksperimental’naja ocenka izmenenij mehanicheskih harakteristik austenitnoj stali v processe jekspluatacii [Computational and experimental evaluation of changes in the mechanical characteristics of austenitic steel during operation]. Nauchnye trudy NIPI Neftegaz GNKAR = Scientific works of NIPI Neftegaz SOCAR, 2019, no 4, pp. 67–72.
2. Zavorin A. S., Makeev A.A., Ljubimova L. L., Tashlykov A.A. Rentgenodilatometricheskie temperaturnye issledovanija stenki kotel’noj truby [X‑ray dilatometric temperature studies of the boiler pipe wall]. Izvestija Tomskogo politehnicheskogo universiteta = News of Tomsk Polytechnic University, 2006, vol. 309, no. 5, pp. 103–106.
3. Landau P., Shneck R. Z., Makov G., Venkert A. Evolution of dislocation patterns in fee metals. Mater. Sci. Engng, 2009, vol. 3, p. 012004.
4. Liu B., He L. Y., Cao Y. The axial crack testing model for long distance oil‑gas pipeline based on magnetic flux leakage internal inspection method. Measurement, 2017, vol. 103, pp. 275–282.
5. Pilipenko S. V. Teoreticheskie osnovy holodnoj pil’gernoj prokatki trub [Theoretical foundations of cold pilger pipe rolling]. Novopolock, Polockij gos. un‑t im. Evfrosinii Polockoj Publ., 2022, 288 p.
6. Klimenko P. L. Uprochnenie stali pri gorjachej deformacii [Hardening of steel during hot deformation]. Dnepropetrovsk, Porogi Publ., 2009, 103 p.
7. Shahabov M. M., Sivenkov A. B., Korol’chenko D.A. Jekspluatacionnye harakteristiki stal’nyh konstrukcij dlitel’nogo sroka jekspluatacii [Operational characteristics of long‑life steel structures]. Vestnik MGSU = MGSU Bulletin, 2023, vol. 18, no. 6, pp. 864–879.
8. Mahutov N.A. Bezopasnost’ Rossii. Pravovye, social’no‑jekonomicheskie i nauchno‑tehnicheskie aspekty. Bezopasnost’ sredstv hranenija i transporta jenergoresursov [Russia’s security. Legal, socio‑economic, scientific and technical aspects. Safety of energy storage and transport facilities]. Moscow, MGOF «Znanie» Publ., 2019, 928 p.
9. Ababkov N. V. Metodologija prognozirovanija i ocenki ostatochnogo resursa konstrukcionnoj i hromomolibdenovanadievyh stalej s primeneniem strukturno‑mehanicheskogo kriterija: dis. … dokt. tekhn. nauk [Methodology for forecasting and estimating the residual life of structural and chromium‑molybdenum‑vanadium steels using a structural and mechanical criterion: dis. … doc. tech. sciences]. Tomsk, 2024, 300 p.
Review
For citations:
Pilipenko S.V., Dudan A.V., Shtempel O.P., Vigerina T.V. Changing the mechanical characteristics of cracking pipes during their long‑term operation. Litiyo i Metallurgiya (FOUNDRY PRODUCTION AND METALLURGY). 2025;(2):64-70. (In Russ.) https://doi.org/10.21122/1683-6065-2025-2-64-70