DETERMINATION OF THE CEMENTED LAYER THICKNESS OF CHROME-NICKEL STEELS
Abstract
It is shown that the thickness of cemented layer defined after cementation by samples from steel 12Хн3А, is overstated by 0,20–0,35 mm because of higher content of nickel.