INFLUENCE OF STRUCTURAL DISPERSION AND COPPER CONTENTS ON FRICTION DURABILITY OF EUTECTIC ANTIFRICTION SILUMIN AK 15

Abstract

It is shown that antifriction silumin with 15% silicon content has maximal frictional endurance in friction pair with steel at 3% copper content and dispersion of globular silicon crystals 3-4 micrometer.

About the Authors

V. Ju. Stetsenko
Institute of Technology of Metals of the NAS of Belarus
Belarus


A. I. Rivkin
Institute of Technology of Metals of the NAS of Belarus
Belarus


K. N. Baranov
Institute of Technology of Metals of the NAS of Belarus
Belarus


References

1. МаруковичЕ. И., Стеценко В. Ю. Модифицирование сплавов. Мн.: Беларуская навука, 2009.

2. Стеценко В. Ю., Ривкин А. И. Новый антифрикционный силумин АК15М3 // Литье и металлургия. 2009. № 3. С. 114–115.


Review

For citations:


Stetsenko V.J., Rivkin A.I., Baranov K.N. INFLUENCE OF STRUCTURAL DISPERSION AND COPPER CONTENTS ON FRICTION DURABILITY OF EUTECTIC ANTIFRICTION SILUMIN AK 15. Litiyo i Metallurgiya (FOUNDRY PRODUCTION AND METALLURGY). 2010;(3):59-61. (In Russ.)

Views: 460


Creative Commons License
This work is licensed under a Creative Commons Attribution 4.0 License.


ISSN 1683-6065 (Print)
ISSN 2414-0406 (Online)